Technical Characteristics: Synthetic artificial graphite with modified performance. High specific capacity, high
first efficiency and long life cycle.
General Characteristics
1. Composition: Graphite
2. Appearance: Black or grey color, no agglomeration, no sundries
Technical Data
Property Unit Typical Value Test Method
PSD D50 µm 15.048 Mastersizer 2000E
Tap density g/cm3 1.30 GB/T 5162
Moisture % 0.03 GB/T 3521
Ash % 0.01 GB/T 3521
FC % 99.99 GB/T 3521
SSA m2/g 1.02 BET
True density g/cm3 2.21 Ultrapyc 1200e
Graphitisation % 95.6 XRD
First discharge capacity mAh/g 355.6 0.2C/Half cell / SBR+CMC
First efficiency % 94.2
Synthetic Artificial Graphite
PGPT203
PDS Targray High Rate Capability Synthetic Artificial Graphite PGPT203 Rev 1.0 2015.04.07”
Synthetic Artificial Graphite PGPT203
Particle Size Distribution
Application
 Soft pack, high capacity aluminium-can, polymer LiB and LiB for EV use
 PVDF and SBR/CMC system
 Capacity up to 340-345mAh/g (pure powder) in cell
 Electrode compressed density 1.60-1.65g/cm3

Synthetic Artificial Graphite for lithium-ion batteries

  • 1.
    Technical Characteristics: Syntheticartificial graphite with modified performance. High specific capacity, high first efficiency and long life cycle. General Characteristics 1. Composition: Graphite 2. Appearance: Black or grey color, no agglomeration, no sundries Technical Data Property Unit Typical Value Test Method PSD D50 µm 15.048 Mastersizer 2000E Tap density g/cm3 1.30 GB/T 5162 Moisture % 0.03 GB/T 3521 Ash % 0.01 GB/T 3521 FC % 99.99 GB/T 3521 SSA m2/g 1.02 BET True density g/cm3 2.21 Ultrapyc 1200e Graphitisation % 95.6 XRD First discharge capacity mAh/g 355.6 0.2C/Half cell / SBR+CMC First efficiency % 94.2 Synthetic Artificial Graphite PGPT203
  • 2.
    PDS Targray HighRate Capability Synthetic Artificial Graphite PGPT203 Rev 1.0 2015.04.07” Synthetic Artificial Graphite PGPT203 Particle Size Distribution Application  Soft pack, high capacity aluminium-can, polymer LiB and LiB for EV use  PVDF and SBR/CMC system  Capacity up to 340-345mAh/g (pure powder) in cell  Electrode compressed density 1.60-1.65g/cm3