The document provides guidelines for the time and temperature settings for laminating EVA glass interlayer films of various thicknesses. It lists the recommended low and high temperature stages and durations for EVA films ranging from 3mm to 11mm thick. Notes specify that a vacuum should be applied before heating and that times should be increased by 10 minutes for tempered glass.