The document describes the synthesis of poly indole through a process involving the mixing of indole crystals, ethanol, water, and ferric chloride for 24 hours to induce polymerization. The resulting polymerized material is then washed through vacuum filtration with ethanol to neutralize the solution. The washed material is dried in a vacuum oven at 90°C for 24 hours then ground into a powder. This powder can then be mixed with DMSO and a binder to prepare an electrode depositing material.