3. CLADDING OF STONE/
VANDEX BITUMINIOUS FELT.
Easy& Fast application (even when wet) Very Slow application and time
No Protection needed (Cost saving). consuming.
Long Life Protection needed (Extra cost)
Forms part of Structural Extra cost of protection
concrete. Does not form part of structure.
Crack Bridge by crystallization upto Has very Limited crack bridging
0.3 mm .
capacity.
Sealmess and no fear of joint failures
due to age. Vandex Super is part Fear of Joint failure ever present due
and parcel of the structural concrete to water pressure or age or poor
incase of structural alterations there workmanship
are no cold joints formed due to age Does not form part of structural
of applications. failure the system is not repairable
Can be applied with ease from from negetive side.
negative side of basement structure Can not be applied or used from
and can be applied post construction
negetive side or post construction.
also.
12. Surface preparation
All concrete to be treated must be
clean and have an ”open” capillary
system.
Remove laitance, dirt, grease, etc. by
suitable means.
20. Three elements of a
successful
Vandex application
1. Surface preparation
2. Product application
21. Application of Vandex products
Prewatering
Surfaces must be carefully prewatered
prior to the Vandex application.
The concrete surface must be damp
but not wet.
23. Do not apply the products at temperatures
below the values indicated on the product
data sheet or on frozen substrates
24. Do not apply the products at temperatures
below the values indicated on the product
data sheet or on frozen substrates
Control of material consumption in
relation to the surface => correct layer
thickness
25. Do not apply the products at temperatures
below the values indicated on the product
data sheet or on frozen substrates
Control of material consumption in
relation to the surface => correct layer
thickness
When problems arise, stop the application
and investigate => damage limitation
26. Do not apply the products at temperatures
below the values indicated on the product
data sheet or on frozen substrates
Control of material consumption in
relation to the surface => correct layer
thickness
When problems arise, stop the application
and investigate => damage limitation
Record batch number of applied material
27. Mixing
Place in a clean container and stir for at least 3
minutes with a mechanical mixer.
28. Mixing
Place in a clean container and stir for at least 3
minutes with a mechanical mixer.
The mixing times have to be respected
precisely !
29. Mixing
Place in a clean container and stir for at least 3
minutes with a mechanical mixer.
The mixing times have to be respected
precisely !
The amount of water may – depending on
environmental conditions and batch variations –
differ slightly from the specified quantity.
30. Mixing
Place in a clean container and stir for at least 3
minutes with a mechanical mixer.
The mixing times have to be respected
precisely !
The amount of water may – depending on
environmental conditions and batch variations –
differ slightly from the specified quantity.
If the mix stiffens, re-mix, do NOT add more
water!