This slide about sewing problem. Generally a lot of way sewing problem occurred. From this slide you guys can learn about some sewing problem & how it's occurred .
5. Fabric Damage
• A garment product can be rejected due to
damage of fabrics or yarn of fabrics in
the seam line. This is mainly happening due
to wrong needle selection or needle damaging
problem. Fabric may be also damaged in case
of new and fine needles due to wrong
selection of needle size and needle point.
6. Types of Fabric Damage
1.Mechanical Damage
2.Needle heating Damage
7. Mechanical Damage
Mechanical damage is the common in apparel
industry. This damaging of fibers or yarns in
the fabrics by needle is the entire faults of
mechanical damage. Mechanical problem is
the main reason for producing defective
fabric.
10. Causes of Mechanical Damage
Inadequate fabric finishing
Damage needle point or throat plate
Mismatch between needle size & throat plate
11. Remedies of Mechanical Damage
Application
of lubricant
along the
stitch line
before
sewing
12. Continue
• The speed of sewing machine should be
reduced.
• Needle size and point should be properly
selected and needle should be free from fault.
• To test the Sew ability before sewing of fabrics
13. Needle Heating Damage
The temperature in needle due to friction
between needle and fabric is up to 300 ºC –
350 ºC. Needle and fabric both may be
damaged in this temperature.
15. Continue
Needle heat is the result of the friction between the
needle and the fabric during
sewing. The following factors can impact the
amount of heat that is generated:
* Thicker fabrics
* Fabrics with harsher finishes or greater density
* Fabric color or density
* Higher sewing machine speeds
16. Continued
* Needle contact surface
− Larger Needle Sizes have more contact area
− Longer Needle Types have more contact area
− Single grooved needle has more contact area
than double
grooved needles.
− Some needle surfaces generate more friction
than others.
17. Remedies of Needle Heating Damage
• 1. Speed: By reducing
sewing speed so that
there is less generating
of heat to the needle.
But, for large
production this is not
granted.
18. Continue
2 . Special type of
needle:
Teflon coated needle
which has extra
smoothness than
galvanized nickel coated
needle may be used to
reduce temperature.
19. Continue
3. Needle Size and Shape: By changing needle
size, shape and use finer needle so that there
is less generation of heat to the needle.
4. Short Length of sewing: The temperature
generation in needle can be reduced by
sewing of short length instead of long length.
20. CONTINUE
5. Cool Air: By
flowing cool air on
the needle during
sewing so that the
temperature can
be controlled
between 70ºC
22. Conclusion
The identification of fabric damage fault with
image would be clear. It is one of the major
problem during sewing . Most of the defects
occur due to improper needle size, pressure
foot adjustment, throat plate replace etc. If
sewing process can be improved, the quality
of the products will be better.