VIP Call Girls Service Kukatpally Hyderabad Call +91-8250192130
la instrucción de laminación de vidrio inteligente PDLC
1. PDLC smart glass Lamination instruction
1. Glass will need to be bigger than the
PDLC smart film
2. Each side the glass will need to be
3mm bigger than the PDLC Film(As picture)
3. For Example:
Glass Size: 1000mm*2000mm, Then
PDLC Film size: 994mm*1994mm
4. In this way, glass can better protect the PDLC film after lamination, and the finished
product will be more stable.
Smart glass lamination process parameters
Low temperature process parameter:
glass thickness(mm) 60℃ low temperature hold time 80℃ high temperature hold time
4+4mm 30 minute 70 minute
5+5mm 30 minute 70 minute
6+6mm 30 minute 75 minute
8+8mm 30 minute 80 minute
10+10mm 30 minute 90 minute
Note: In low temperature process, it is better for fabric laminated glass, cause some insert materials
can not stand very high temperature. But if make transparent laminated glass, we suggest use high
temperature process.
Notice:
All the data are the test parameters just for reference. The final produce data depends
on the customer data of your own after you test in your own factory.