MS BEAM
We supply an extensive range of MS Beam, developed using
premium quality mild steel. MS Beam helps in ensuring
construction of a sturdy infrastructure, providing maximum lifespan,
also provides resistance against corrosion and high tensile
strength. We deal in MS Beam prepared as per the industrial
standards and are available in various sizes and are offered at
discounted prices.
website: https://shreejisteelcorp.com/
SHREE JI STEEL CORPORATION
Product Name MS Beam
Brand
Features
Application
Minimum Order
Quantity
Place Of Origin
Material
Material Grade
SJ SHREE JI
IS 2062
Mild Steel
Kolkata/Durgapur
16 Metric Ton
Construction
Sturdiness, increasing
infrastructural life, providing
tensile strength.
website: https://shreejisteelcorp.com/
MS Beam Sizes and Weights
Size (in mm)
Weight
(in Kg/m)
Weight
(in Kg/foot)
MS Beam 125 x 70 x 5
MS Beam 150 x 75 x 5
MS Beam 175 x 85 x 5.8
MS Beam 200 x 100 x 5.7
MS Beam 250 x 125 x 6.9
MS Beam 300 x 140 x 7.7
MS Beam 350 x 140 x 8.1
MS Beam 400 x 140 x 8.9
MS Beam 450 x 150 x 9.4
MS Beam 500 x 180 x 10.2
MS Beam 600 x 210 x 12
13.400
15.000
19.600
25.400
37.300
46.100
52.400
61.600
72.400
86.900
123.000
4.084
4.572
5.974
7.742
11.369
14.051
15.971
18.775
22.067
26.487
37.490
website: https://shreejisteelcorp.com/
Rolling Tolerances of MS Beam
Depth Tolerance Width of flange Tolerance
Up to 200 mm
> 200 to 400 mm
± 2.5 mm
± 3.0 mm
Up to 100 mm ± 2 mm
Tolerance on weight per meter shall be ± 2.5% or alternatively +4, -1% of the
standard weight per meter. The permissible limits for camber and sweep shall
be 0.2% of the length.
website: https://shreejisteelcorp.com/
MS Beam Chemical Composition: (in % max
values)
Tolerance
Carbon
%
Manganese
Max %
Sulphur
Max %
Phosporous
Max %
Silicon
Max %
Carbon
Equivalent
0.23
+0.02
1.50 0.045 0.045 0.40 0.42
+0.05 +0.005 +0.005 +0.03 +0.03
MS Beam Mechanical Composition: (in % max
values)
Tensile
Strength
Min, Mpa
Yield Stress, Min, MPa
% Elongation at
gauge length
5.65 √Ѕo
Bend Test
mm
410
<20
mm
250
20-40 mm
240
>40
mm
230
min
23
min
3t* (*t is 3
times
thickness)
website: https://shreejisteelcorp.com/

MS Beam

  • 1.
    MS BEAM We supplyan extensive range of MS Beam, developed using premium quality mild steel. MS Beam helps in ensuring construction of a sturdy infrastructure, providing maximum lifespan, also provides resistance against corrosion and high tensile strength. We deal in MS Beam prepared as per the industrial standards and are available in various sizes and are offered at discounted prices. website: https://shreejisteelcorp.com/ SHREE JI STEEL CORPORATION
  • 2.
    Product Name MSBeam Brand Features Application Minimum Order Quantity Place Of Origin Material Material Grade SJ SHREE JI IS 2062 Mild Steel Kolkata/Durgapur 16 Metric Ton Construction Sturdiness, increasing infrastructural life, providing tensile strength. website: https://shreejisteelcorp.com/
  • 3.
    MS Beam Sizesand Weights Size (in mm) Weight (in Kg/m) Weight (in Kg/foot) MS Beam 125 x 70 x 5 MS Beam 150 x 75 x 5 MS Beam 175 x 85 x 5.8 MS Beam 200 x 100 x 5.7 MS Beam 250 x 125 x 6.9 MS Beam 300 x 140 x 7.7 MS Beam 350 x 140 x 8.1 MS Beam 400 x 140 x 8.9 MS Beam 450 x 150 x 9.4 MS Beam 500 x 180 x 10.2 MS Beam 600 x 210 x 12 13.400 15.000 19.600 25.400 37.300 46.100 52.400 61.600 72.400 86.900 123.000 4.084 4.572 5.974 7.742 11.369 14.051 15.971 18.775 22.067 26.487 37.490 website: https://shreejisteelcorp.com/
  • 4.
    Rolling Tolerances ofMS Beam Depth Tolerance Width of flange Tolerance Up to 200 mm > 200 to 400 mm ± 2.5 mm ± 3.0 mm Up to 100 mm ± 2 mm Tolerance on weight per meter shall be ± 2.5% or alternatively +4, -1% of the standard weight per meter. The permissible limits for camber and sweep shall be 0.2% of the length. website: https://shreejisteelcorp.com/
  • 5.
    MS Beam ChemicalComposition: (in % max values) Tolerance Carbon % Manganese Max % Sulphur Max % Phosporous Max % Silicon Max % Carbon Equivalent 0.23 +0.02 1.50 0.045 0.045 0.40 0.42 +0.05 +0.005 +0.005 +0.03 +0.03 MS Beam Mechanical Composition: (in % max values) Tensile Strength Min, Mpa Yield Stress, Min, MPa % Elongation at gauge length 5.65 √Ѕo Bend Test mm 410 <20 mm 250 20-40 mm 240 >40 mm 230 min 23 min 3t* (*t is 3 times thickness) website: https://shreejisteelcorp.com/