Sputtering
&
Thin Film Deposition
Thin Film Applications
• Window coatings
• Magnetic media
• Semiconductors
• Biomedical devices
• Optics
• Automotive
• Aerospace
http://spectrum.ieee.org/energy/renewables/first-solar-quest-for-the-1-watt/0
Deposition Processes
• Evaporation (thermal)
• Sputter deposition (DC, RF, PE)
• CVD, MO-CVD, PE-CVD
• Plasma polymerized films
• Solution cast (spin coating) films
• Self Assembled Monolayers
(SAMs)
Thin Film Deposition
– Need other types of films besides SiO2
– insulating films for GaAs & III-V
• Oxide no good
• Need SiO2 or Si3N4
– Need metal lines for electrical connects
– Need insulation for these metal wires
– Need to deposit other types of semiconductors
• Heterostructures, epitaxy
• 2 categories
1. Physical vapor deposition
2. Chemical vapor deposition
Physical Vapor Deposition (PVD)
1. Evaporation (8.1.1)
• Simplest case
• Evaporate metal to gaseous state (↑T) by heat or e-
beam
• Evaporated atoms float up to the wafer and condense on cool wafer surface
• Equivalent to boiling water and condensation onto pot lid
• Solid – usually polycrystalline
• Characteristics (film)
• Usually low melting point materials  metals
• Must be pure (different Tm / vapor pressure)
• Can have multiple sources but difficult to control relative fluxes
• Atoms move by line of sight
• Straight shot from source to wafer
• Shadowing effects
• Masking, poor step coverage
• Poor uniformity  spin wafers
heat
metal
source
wafer
evacuated
chamber
e-
beam
localized heating
- less contamination from
crucible
Evaporation
Vacuum Requirements
 Purity of film
 Must have large mean free path (distance
before collision with some molecule)
2
2 d
P
T
k c
B





T – usually room temp. of chamber (?)
P = pressure of chamber
D = diameter of vapor atom ~2-5 Å
for P ~ 10-4
Pa  λ ~ order of meters
Atoms into Gas State
• At target:
– target atoms ejected
– target ions ejected (1 - 2 %)
• Electrons emitted
– helps keep plasma going
• Ar+ ions reflected as Ar neutrals
• Ar buried in target
• Photons emitted
Vacuum Deposition
Physical Vapor Deposition
• Evaporation [ HV, UHV,
Inert Gas Reactive]
• Sputtering [ HV, UHV,
Inert Gas, Reactive]
• Pulsed Laser
Deposition [HV, UHV,
Inert Gas, Reactive ]
Chemical Vapor Deposition
• Thermal Growth
[Plasma Assisted ]
• Polymerization
• Plasma assisted
• Chemical growth
• Plasma enhanced
Sputter Deposition
– energy of Ar+
~10eV – 10keV
• not as high as ion implantation but still enough to mechanically
impact target and knock off atoms.
• called sputtering  sputter etch / ion milling
– purely mechanical
– sputtered atoms (generally neutral ) diffuse down to anode and
deposit there
– anode = substrate
– cathode = desired film material
– okay for conductive substrates and targets, but not for insulators
• charge builds up at cathode
 RF (radio frequency) sputtering
Ar
Gas Flow Sputtering
Comparison of Evaporation vs.
Sputtering Process and Films
Comparison of evaporation and sputtering
EVAPORATION SPUTTERING
low energy atoms higher energy atoms
high vacuum path
 few collisions
 line of sight deposition
 little gas in film
low vacuum, plasma path
 many collisions
 less line of sight deposition
 gas in film
larger grain size smaller grain size
fewer grain orientations many grain orientations
poorer adhesion better adhesion
DC Sputtering
DC Sputter
Deposition
Sputter deposition is a
physical vapor deposition (PVD) method of
depositing thin films by sputtering, that is
ejecting, material from a "target," source,
which then deposits onto a "substrate," such
as a silicon wafer. Sputtered atoms ejected
from the target have a wide energy
distribution, typically up to tens of eV (100,000
K). The sputtered ions (typically only a small
fraction (~1% of the ejected particles are
ionized) can ballistically fly from the target in
straight lines and impact energetically on the
substrates or vacuum chamber (causing
resputtering). Energetic ions sputter material
off the target which diffuse through the plasma
towards the substrate where it is deposited.
There is no strong plasma glow around the
cathode since it takes a certain distance for
the plasma to be generated by electron
avalanches started by a few secondary
electrons from the sputtering process.
http://en.wikibooks.org/wiki/Microtechnology/Additive_Processes
Chemical Vapor Deposition
– consists of precursors reacting at surface to
form film
• e.g. electronic grade Si
– SiHCl3  Si + HCl
• e.g. SiO2
– SiH4 (g) + O2 (g)  SiO2 + H2
– can get epitaxial growth [vapor phase epitaxy
(5.3)]
• same differences apply ↓Φ, ↑T
Chemical Vapor Deposition
Steps
1. transport of reactants to wafer
2. transfer of reactants from gas stream to
substrate surface
3. reactants adsorb onto surface
4. chemical reaction / surface diffusion
5. incorporation (for epitaxy)
6. desorption of byproducts
Rate limiting steps (slowest)
1. transport of reactant to substrate
2. chemical reaction at surface
precursors
wafer
exhaust
Chemical Vapor Deposition
III-Vs
• GaAs
1. ease of “cracking” precursor too early
2. byproducts are harmful
3. purity
4. toxicity
– Halide process
AsCl3 + H2  As4 + HCl
Ga + As  GaAs
GaAs + HCl  GaCl + As
dep. GaAs on substrate
– other precursors
– Metal Organics (MOCVD)
– TM_____ trimethyl  ex. Ga(CH3)3
– TE_____ triethyl  ex. Ga(C2H5)3
– TMGa + AsH3  GaAs + CH4 ~600°C - 800°C
– can flow in In + Ga to make alloy
– composition of alloy determined by relative flux
– can get C contamination
Spin Coat
Spin coating is a procedure used to apply
uniform thin films to flat substrates. In
short, an excess amount of a solution is
placed on the substrate, which is then
rotated at high speed in order to spread the
fluid by centrifugal force. A machine used
for spin coating is called a spin coater, or
simply spinner. Rotation is continued while
the fluid spins off the edges of the
substrate, until the desired thickness of the
film is achieved. The applied solvent is
usually volatile, and
simultaneously evaporates. So, the higher
the angular speed of spinning, the thinner
the film. The thickness of the film also
depends on the concentration of the
solution and the solvent. Spin coating is
widely used in microfabrication, where it
can be used to create thin films with
thicknesses below 10 nm. It is used
intensively inphotolithography, to deposit
layers of photoresist about
micrometer thick. http://en.wikipedia.org/wiki/Spin_coating
Characterization Tools
• SEM-EDX
– Imaging
– X-Ray Analysis
• XPS/AES
– Elemental composition
– Chemical bonding
– Depth composition
profiles
• XRF
– Composition
– Film thickness
• XRD
– Crystal structure
– Phase
• TEM
– Imaging
– Atomic structure